All the details- Low silver, high fluidityUnited's own description for #543, which helps it fill fine detail cleanly when cast.
- All-purposeUnited publishes separate casting and fabrication instructions for the same alloy, covering wire, sheet and plate work too.
- Nickel-free0.00% nickel in United's published composition, unlike our nickel-based white alloys.
- Covers 9K to 18KFrom a single dark pink alloy.
European Design's #543 Dark Pink is United Precious Metal Refining's all-purpose master alloy for 9K through 18K pink gold: low silver and high fluidity, equally suited to casting or to working into wire, sheet and plate. Melt it with fine gold and cast or fabricate as usual.
Mixing ratio by karat
| Karat | Fine gold (by weight) | Master alloy (by weight) |
|---|---|---|
| 9K | 37.5% | 62.5% |
| 14K | 58.5% | 41.5% |
| 18K | 75.0% | 25.0% |
Fine-gold percentages are standard karat fineness, independent of the alloy maker.
| Maker | United Precious Metal Refining |
|---|---|
| Karat range | 9K-18K |
| Colour | Dark pink |
| Use | All-purpose — casting and fabrication (wire, sheet, plate) |
| Composition | Copper 92.50%, silver 4.50%, zinc 3.00%, nickel 0.00% (nickel-free; no palladium) |
| Melting range | 1,040-1,050°C (1,904-1,922°F) pre-alloying; 980-1,055°C (1,796-1,931°F) casting, by karat |
| Alloying ratio | 37.5% fine gold for 9K, 58.5% for 14K, 75.0% for 18K, by weight |
| Sold as | By weight, 50 g - 1,000 g (1 kg) |
| Made in | USA |
Sold as
By weight: order 50 g, 100 g, 500 g or 1,000 g (1 kg) of alloy grain. Fine gold is not included — melt it in yourself to reach the karat you need.
Good to know
- Casting quench depends on karat: 9-14K pieces quench after a 15-minute cool; for 18K, cool the button 3 minutes first, then quench.
- Fabricating an ingot: melt the alloy in the bottom of the crucible with fine gold on top, then pour into a preheated mould — a round rod mould for wire, a 2-piece L-shaped mould for sheet or plate.
- Roll or draw in 50% steps, annealing at 704°C (1,300°F) for 20 minutes between passes; over-annealing causes grain growth and an orange-peel surface.
- Don't confuse this with Legor's Pink Master Alloy: both are dark pink/red 9K-and-up alloys, but #543 is United's nickel-free formulation, while Legor's OR134 is a separate recipe.