Legor Pink Master Alloy
Price on request
Shipped across CanadaBy courier or freight: we quote delivery with your price.
Features
All the details- Our widest karat rangeUse this one alloy for 9K, 14K, 18K, 21K and 22K.
- Very high grain refinementLegor's own rating, which helps avoid the brittleness that can affect traditional 18K red gold.
- All-purposeSuits lost-wax casting, with or without stones in place, as well as wire, sheet and tube work.
- Nickel-freeCopper, silver and zinc only — no nickel in Legor's published composition.
European Design's LEGOR Pink Master Alloy (OR134) is Legor Group's all-purpose master alloy for 9K through 22K red/pink gold - Legor's own colour name for it is "Red". Melt it with fine gold, then cast it (with or without stones in place) or work it into wire, sheet or tube.
Mixing ratio by karat
| Karat | Fine gold (by weight) | Master alloy (by weight) |
|---|---|---|
| 9K | 37.5% | 62.5% |
| 14K | 58.5% | 41.5% |
| 18K | 75.0% | 25.0% |
| 21K | 87.5% | 12.5% |
| 22K | 91.7% | 8.3% |
Karats and per-mille figures are Legor's own stated range for OR134. Fine-gold percentages are standard karat fineness.
| Maker | Legor Group |
|---|---|
| Karat range | 9K-22K |
| Colour | Pink (Legor's own colour name for OR134 is "Red") |
| Use | All-purpose — lost-wax casting and fabrication (wire, sheet, tube) |
| Composition | Copper 93.0%, silver 5.0%, zinc 2.0% (nickel-free; no palladium) |
| Melting range | 950-985°C (1,742-1,805°F), solidus-liquidus |
| Alloying ratio | 37.5% fine gold for 9K, up to 91.7% for 22K, by weight |
| Sold as | By weight, 100 g |
| Made in | Italy |
Sold as
Each: 100 g of Legor OR134 casting grain. Fine gold is not included — melt it in yourself to reach the karat you need.
Good to know
- Casting without stones: pull the flask within 1 minute of pouring and quench directly in water; with stones in place, let the flask cool 30-45 minutes first.
- Pickle at a gentle temperature: a 50 g/l RADIAL solution at 60°C (140°F) for 2 minutes, or 10% sulphuric acid at 50°C (122°F) for 5 minutes.
- Draw and roll in stages: wire can be drawn 45% in diameter and sheet reduced 70% in area before annealing at 620-660°C (1,148-1,220°F).
- Don't confuse this with our other dark pink alloy: Dark Pink All-Purpose Alloy (9K-18K) is United Precious Metal Refining's #543, a separate nickel-free recipe.