Skip to product information
Item no. 10-473-50Sold by quote
Rich Reddish Yellow Casting Alloy (9K-14K Ultra Alloy)
Price on request
Shipped across CanadaBy courier or freight: we quote delivery with your price.
Features
All the details- Reddish tone from copperAt 65% copper, the largest share of the formula, this alloy casts a warmer, redder yellow than a standard alloy.
- Built for stone-in-place castingUnited PMR markets UA1 for high reusability and tarnish resistance when casting with stones already set.
- Hardens with the karatAs-cast hardness rises from 152 HV at 10K to 165 HV at 14K, per United PMR's technical sheet.
- Made by United PMR(Alden, New York), a full-service precious-metal refiner.
United PMR's UA1, sold as the Ultra Alloy, is a 9K-14K master alloy grain: melt it with fine gold to cast a rich, reddish yellow. Its high copper content gives the warm tone, and United PMR markets it for high reusability and tarnish resistance, including stone-in-place casting. Sold by weight in 50 g, 100 g, 500 g and 1 kg quantities.
Casting reference by karat (United PMR data)
| Karat | Casting temperature | Density | As-cast hardness (HV) |
|---|---|---|---|
| 10K | 935-955 °C (1,715-1,751 °F) | 11.58 g/cc | 152 |
| 14K | 920-940 °C (1,688-1,724 °F) | 13.05 g/cc | 165 |
Pre-alloying 1,040-1,050 °C (1,910-1,925 °F); flask 510-650 °C (950-1,202 °F); quench 15-20 minutes; remelt with up to 50% fresh mix.
| Maker | United Precious Metal Refining, Inc. (United PMR), Alden, NY |
|---|---|
| Product code | UA1 (Ultra Alloy) |
| Colour | Rich Reddish Yellow |
| Karat range | 9K-14K |
| Form | Alloying grain |
| Use | Casting |
| Composition | Copper 65%, silver 23%, zinc 12%, nickel 0% |
Sold as
By weight: 50 g, 100 g, 500 g or 1 kg. Fine gold is not included; melt in the karat and quantity of fine gold you need separately.
Good to know
- This is the base-metal portion only. Melt the right weight of fine gold into it to reach the karat you want; 14K needs 585 g of fine gold per kilogram of finished alloy, with this master alloy making up the other 415 g.
- Flux sparingly. United PMR recommends very little boric acid flux, no carbon flux such as soda ash or saltpetre, and none at all in a bottom-pour automatic casting unit.
- Use gypsum-bonded investment and follow its maker's burnout cycle; a fluoric-based investment remover clears the silicon-oxide surface coating better than an aggressive acid, which can corrode the casting.
- Working out how much to melt: multiply the alloy's density by the wax pattern's weight in grams, then add 10% for the button.
Need help choosing?Tell us what you’re making and we’ll point you to the right size and item number.