Skip to product information
Item no. 10-472-50Sold by quote
Rich Yellow Casting Alloy (9K-14K)
Price on request
Shipped across CanadaBy courier or freight: we quote delivery with your price.
Features
All the details- Built for stone-in-place castingUnited PMR markets 280 for high reusability and tarnish resistance when casting with stones already set.
- Nickel-freeThis alloy contains no nickel, unlike our Standard Yellow (210) master alloy.
- Consistent 9K-14K performanceAs-cast hardness holds close across the range: 151 HV at 10K, 152 HV at 14K, per United PMR's technical sheet.
- Made by United PMR(Alden, New York), a full-service precious-metal refiner.
United PMR's 280 is a 9K-14K master alloy grain: melt it with fine gold for a rich yellow casting alloy. United PMR markets it for high reusability and tarnish resistance, including stone-in-place casting, and it's nickel-free. Sold by weight in 50 g, 100 g, 500 g and 1 kg quantities.
Casting reference by karat (United PMR data)
| Karat | Casting temperature | Density | As-cast hardness (HV) |
|---|---|---|---|
| 10K | 935-955 °C (1,715-1,751 °F) | 11.5 g/cc | 151 |
| 14K | 915-935 °C (1,679-1,715 °F) | 13.01 g/cc | 152 |
Pre-alloying 1,010-1,040 °C (1,850-1,910 °F); flask 510-650 °C (950-1,202 °F); quench 15-20 minutes; remelt with 35-50% fresh mix.
| Maker | United Precious Metal Refining, Inc. (United PMR), Alden, NY |
|---|---|
| Product code | 280 |
| Colour | Rich Yellow |
| Karat range | 9K-14K |
| Form | Alloying grain |
| Use | Casting |
| Composition | Copper 68%, silver 23%, zinc 9%, nickel 0% |
Sold as
By weight: 50 g, 100 g, 500 g or 1 kg. Fine gold is not included; melt in the karat and quantity of fine gold you need separately.
Good to know
- This is the base-metal portion only. Melt the right weight of fine gold into it to reach the karat you want; 14K needs 585 g of fine gold per kilogram of finished alloy, with this master alloy making up the other 415 g.
- Flux sparingly. United PMR recommends very little boric acid flux, no carbon flux such as soda ash or saltpetre, and none at all in a bottom-pour automatic casting unit.
- Use gypsum-bonded investment and follow its maker's burnout cycle; a fluoric-based investment remover clears the silicon-oxide surface coating better than an aggressive acid, which can corrode the casting.
- Working out how much to melt: multiply the alloy's density by the wax pattern's weight in grams, then add 10% for the button.
Need help choosing?Tell us what you’re making and we’ll point you to the right size and item number.