Skip to product information
Features
All the details- Made for resin prints(DLP and SLA) as well as injection waxes, carving waxes, wax-based polymers and hybrid wax/plastic patterns.
- Handles a full resin burnoutIt withstands up to 830 °C (1,526 °F).
- 8-minute working timeWith an automatic vacuum investing machine or a conventional mixer and vacuum.
- Recommended by resin makersFormlabs (Castable Wax and Castable Wax 40) and BlueCast.
- Made by Certus
Certus Prestige OPTIMA is a gypsum-bonded investment made to burn out 3D-printed resin patterns cleanly, and it works with waxes too. It's the investment Formlabs recommends for its Castable Wax resins, and one of BlueCast's top picks for detail and surface finish. Sold in Certus's 49.6 lb (22.5 kg) plastic drum.
Mixing table (Certus)
| Method | Water per 1 kg | Water per 1 lb | Working time |
|---|---|---|---|
| Automatic vacuum investing machine | 380 ml | 172 ml | 8 min |
| Conventional mixer + vacuum | 400 ml | 182 ml | 8 min |
| Resin prints, lighter designs | 380 ml | 172 ml | 8 min |
| Resin prints, larger or thicker designs | 370 ml | 168 ml | 8 min |
Each 1% of extra powder shortens the working time by about 30 seconds, so weigh both accurately.
| Maker | Certus (Prestige) |
|---|---|
| Type | Gypsum-bonded investment |
| For | 3D-printed resin (DLP/SLA) and wax patterns |
| Water : powder | 38–40 ml per 100 g for wax; 37–38 ml per 100 g for resin prints |
| Water | 21–24 °C (70–75 °F), distilled or de-ionised |
| Working time | 8 minutes |
| Bench set before burnout | 90–120 min for wax; at least 3–4 h for resin |
| Maximum burnout | 830 °C (1,526 °F) |
| Pack | 49.6 lb (22.5 kg) net of powder in a plastic drum with lid |
| Packed for shipping | About 55 lb (24.9 kg); about 13 × 13 × 11 in (33 × 33 × 28 cm) |
| Made in | Turkey |
Sold as
Each: one 49.6 lb (22.5 kg) Certus plastic drum.
Good to know
- Resin burnout, Certus method A: hold at 100 °C (212 °F) for 2–4 h to drive off the water, then ramp quickly to peak.
- Resin burnout, method B: load into an oven preheated to 500 °C (932 °F) for 3–4 h, ramp quickly to a peak of up to 780 °C (1,436 °F) and hold up to 5 h, then drop to flask temperature and hold 2 h before casting.
- Wax burnout (Certus's published cycle): 150 °C (302 °F) for 3 h, 370 °C (698 °F) for 2 h, 750 °C (1,382 °F) for 4 h, then down to casting temperature.
- Turn the flask sprue-up while the kiln comes down to casting temperature.
- Troubleshooting: too much water gives rough surfaces and flashing; too little traps air bubbles.
Contains crystalline silica. Don't breathe the dust: mix under local exhaust, and wear a fine-particle dust mask (FFP3 or N100 class) and eye protection when pouring and mixing. Not regulated for transport.
Need help choosing?Tell us what you’re making and we’ll point you to the right size and item number.