ALL 2000 Platinum Investment
Often bought together
What jewellers take with this, in the size they usually choose.
Features
All the details- Built for platinum pressure castingA 100% silica investment with Yoshida's own binder, made for pressure-cast platinum and palladium.
- Withstands up to 950 °CFar higher than a gypsum investment, to survive platinum's much higher pour temperature.
- Mixed with Cast LiquidYoshida's own binder diluted with water, at 38–40% by weight; about 10 minutes to mix by machine.
- Dehydrates instead of just bench-setting10 hours on a bed of Yoshida ALL 1 powder pulls the water out of the mould before burnout.
- Made by Yoshida CastIn business since 1960.
Yoshida's ALL 2000 is a silica investment made specifically for pressure-casting platinum and palladium, not the gypsum-bonded plaster used for gold. It mixes with Yoshida's own Cast Liquid binder rather than plain water, and withstands burnout up to 950 °C. Sold in Yoshida's 55.1 lb (25 kg) box.
Mixing table (Yoshida)
| Method | Cast Liquid per 1 kg | Cast Liquid ratio | Mixing time |
|---|---|---|---|
| Machine mixing (pressure casting) | 400 ml | 38–40% | About 10 min |
| Hand mixing | 340–370 ml | 34–37% | Until creamy |
Cast Liquid is Yoshida's Platinum Liquid binder diluted with water, not plain water. Below 38% risks a missed fill; a higher ratio can leave a rougher surface.
| Maker | Yoshida Cast Industry Co. |
|---|---|
| Type | Silica investment with proprietary binder, for pressure casting |
| For | Platinum and palladium, pressure casting |
| Binder | Yoshida Cast Liquid (Platinum Liquid concentrate diluted 40 ml to 960 ml water) |
| Cast Liquid : powder | 400 ml per 1 kg powder (38–40% by weight) |
| Mixing time | About 10 minutes by machine |
| Dehydration | 10 hours on a bed of Yoshida ALL 1 powder before burnout |
| Maximum burnout | 950 °C (1,742 °F); do not exceed 1,000 °C or hold over 4 hours |
| Pack | 55.1 lb (25 kg) box |
| Made in | Japan |
Sold as
Each: one 55.1 lb (25 kg) box.
Good to know
- Mix with Cast Liquid, not water: Yoshida's Platinum Liquid binder concentrate diluted with fresh water.
- Use its own equipment: keep a dedicated mixer and containers separate from gypsum investment. The slurry is more viscous and can strain a gypsum-rated mixer's motor, and any gypsum residue baked in above 800 °C can create harmful gas and porosity.
- Invest into an Alma-Ring Flask (we carry it), then dehydrate for 10 hours on a bed of Yoshida ALL 1 powder instead of an ordinary bench-set.
- Burn out in three stages (150 °C, 250 °C, then up to 950 °C). Do not exceed 1,000 °C or hold for more than 4 hours, as this reduces mould permeability.
Contains natural silica dust: work under ventilation and wear a fine-particle dust mask when handling the powder. Hot moulds can crack violently when quenched in water; use eye protection and heat-resistant gloves and keep others clear during stripping.