All the details- Built for the platinum rangeRated for platinum, palladium and stainless steel, beyond what a gypsum-bonded investment can take.
- Binder includedComes with enough binder concentrate to mix the whole pack of powder — nothing extra to buy.
- Special additives cut air bubblesThe cast comes out with a smoother surface that needs less finishing than typical two-part investments.
- Easier to removeBreaks away from the casting more easily than a phosphate-bonded investment.
- From CertusThe Turkish maker behind our Prestige Optima and Prestige Oro investments.
Certus Prestige Ferro-Vest V.H.T. is a two-part, high-temperature investment for casting platinum, palladium and stainless steel: alloys too hot for a gypsum-bonded investment like our Prestige Optima or Prestige Oro. Each pack comes with its own binder concentrate, mixed with water in place of plain water alone. Sold in a 49.6 lb (22.5 kg) pack.
Mixing chart (Certus, per flask)
| Flask size | Powder | Water | Binder concentrate added |
|---|---|---|---|
| 6" x 3.5" flask | 1,500 g (3.3 lb) | 428 cc | 23 cc (33 g) |
| 8" x 3.5" flask | 1,650 g (3.6 lb) | 470 cc | 25 cc (36 g) |
Per-flask amounts from Certus’s chart, which gives combined totals for up to six flasks at a time; amounts scale in direct proportion.
| Maker | Certus (Prestige) |
|---|---|
| Type | Two-part high-temperature investment (powder plus binder concentrate) |
| For | Platinum, palladium and stainless steel; metals melting above 1500°C (2732°F) |
| Binder dilution | 1:19 by volume, binder concentrate to distilled water |
| Powder : solution | 100 parts powder to 28-30 parts diluted solution, by volume |
| Bench set before burnout | 2-3 h for a 4 in flask; up to overnight for an 8 in flask |
| Same-day burnout peak | 870°C (1,600°F) |
| Pack | 49.6 lb (22.5 kg), binder concentrate included |
Sold as
Each: one 49.6 lb (22.5 kg) pack of Ferro-Vest V.H.T. powder, with its binder concentrate included.
Good to know
- Add the binder to the water, not the reverse: 1 part concentrate to 19 parts distilled water.
- Choosing between our investments: Prestige Optima and Prestige Oro are gypsum-bonded investments for gold, palladium and platinum up to 22K with a lower burnout ceiling; Ferro-Vest's two-part system is for platinum, palladium and stainless steel that need a much higher burnout.
- Let it bench-set fully before burnout: 2-3 hours for a 4 in flask, up to overnight for an 8 in flask, then 2 more hours once it feels hard before stripping the rubber base.
- Same-day burnout (small flasks): ramp to 93°C (200°F) and hold 2 h, then 175°C (350°F) for 1 h, then up to 870°C (1,600°F) over 4.5-5 h and hold until the investment turns fully white.
- Pour gently down the flask wall, not directly onto the pattern, and vacuum both the mixed slurry and the poured flask for 1.5-2 minutes each.
The binder concentrate is acidic. Wear eye and hand protection when diluting it, and always add the concentrate to the water, not water to the concentrate.