Skip to product information
Item no. 10-451-50Sold by quote
Pale Light Yellow Casting Alloy (18K)
Price on request
Shipped across CanadaBy courier or freight: we quote delivery with your price.
Features
All the details- Rated for 18KUnited Precious Metal Refining (UPMR) #740 is an 18K casting alloy.
- High tarnish resistance and lustreUPMR formulates #740 for a bright, long-lasting cast surface.
- Needs very little fluxA touch of boric acid is enough; skip carbon-based flux such as soda ash or saltpetre, and a bottom-pour automatic caster needs none at all.
- RemeltableTop up scrap buttons and sprues with 50% fresh alloy and recast.
- Sold by weight50 g, 100 g, 500 g and 1 kg, so small studios and production casters buy the same alloy.
Alloy #740 from United Precious Metal Refining (UPMR) is a pale light yellow master alloy for casting 18K gold: add fine gold and it gives high tarnish resistance and a bright, high-lustre cast surface. It needs very little flux and can be remelted with a 50% top-up of fresh alloy. Sold by weight in 50 g, 100 g, 500 g and 1 kg.
| Maker | United Precious Metal Refining (UPMR) |
|---|---|
| Karat range | 18K |
| Colour | Pale light yellow |
| Use | Casting |
| Composition | Cu 37.5%, Ag 60%, Zn 2.5%, Ni 0% |
| Melting range | 975–995 °C (1,786–1,822 °F) casting; 1,050–1,070 °C (1,922–1,958 °F) pre-alloying |
| Alloying ratio | 750 g fine gold + 250 g alloy per kg (18K) |
| Sold as | 50 g, 100 g, 500 g or 1 kg of alloy grain |
| As-cast hardness | 143 HV |
| Made in | USA |
Sold as
By weight: 50 g, 100 g, 500 g or 1 kg of alloy grain. No gold, flux or investment included.
Good to know
- Flux sparingly. UPMR recommends only a little boric acid; avoid carbon-based fluxes like soda ash or saltpetre, and skip flux entirely in a bottom-pour automatic caster.
- Sizing a pour: multiply the alloy's density by your wax pattern's weight, then add 10% for the button, to work out how much metal to melt.
- Investment: UPMR recommends gypsum-bonded investment, and a fluoric-based investment remover for the silicon-oxide film that forms on this alloy; aggressive acid removers can corrode and mark the surface.
- Quench and remelt: quench 15–20 minutes after casting, and mix any remelted scrap with 50% fresh alloy.
Need help choosing?Tell us what you’re making and we’ll point you to the right size and item number.