Skip to product information
Item no. 10-470-50Sold by quote
White Casting Alloy (9K-14K)
Price on request
Shipped across CanadaBy courier or freight: we quote delivery with your price.
Features
All the details- High silver baseMade of 36.00% copper, 28.00% silver, 20.00% zinc and 16.00% nickel.
- Casts cooler835-855 °C (1,535-1,571 °F) at 10K and 845-865 °C (1,553-1,589 °F) at 14K, some 170-230 °C below United's #940 at the same karat.
- Soft to work, in United's wordsThough it casts harder at 10K (211 HV) than at 14K (163 HV).
- Give it time before quenchingUnited allows 20-30 minutes after casting, and a 50% fresh mix when you remelt.
#943 is United Precious Metal Refining's white master alloy for 9K to 14K white casting gold. It is built on silver, 28% alongside copper, zinc and 16% nickel; United describes it as soft to work, and it casts well below the temperatures of our silver-free #940. Sold by weight as grain, from 50 g to 1 kg.
Casting reference by karat (United PMR data)
| Karat | Fine gold + #943, per 100 g | Casting temperature | Density | As-cast hardness |
|---|---|---|---|---|
| 10K | 41.7 g + 58.3 g | 835-855 °C (1,535-1,571 °F) | 11.45 g/cc | 211 HV |
| 14K | 58.5 g + 41.5 g | 845-865 °C (1,553-1,589 °F) | 12.96 g/cc | 163 HV |
United covers 9K-14K but gives these figures for 10K and 14K; for 9K, use 37.5 g of fine gold with 62.5 g of #943 per 100 g. Fine-gold weights follow standard fineness (375, 417, 585).
| Maker | United Precious Metal Refining |
|---|---|
| Product code | 943 |
| Colour | White |
| Karat range | 9K-14K |
| Form | Alloying grain |
| Use | Investment casting |
| Composition | Copper 36.00%, silver 28.00%, zinc 20.00%, nickel 16.00% (published figures; United adds proprietary metals it doesn't list) |
| Pre-alloying | 1,050-1,060 °C (1,922-1,940 °F) |
| Flask temperature | 540-675 °C (1,004-1,247 °F) |
| Quench and remelt | Quench after 20-30 minutes; remelt with 50% fresh metal |
| Sold as | By weight: 50 g, 100 g, 500 g or 1 kg |
| Made in | USA |
Sold as
By weight: 50 g, 100 g, 500 g or 1 kg of #943 alloy grain. No fine gold, flux or investment included.
Good to know
- This is the alloy, not the gold: you melt it with fine gold to reach your karat. For 100 g of 14K, that is 58.5 g of fine gold and 41.5 g of #943.
- Work out the metal from the wax: multiply the alloy's density by the wax pattern's weight in grams, then add 10% for the button. At 14K the density is 12.96 g/cc.
- Keep the flux to a pinch: a little boric acid is all United calls for. It rules out carbon-based fluxes such as soda ash and saltpetre, and a bottom-pour automatic caster needs none at all.
- Investing and devesting: use a gypsum-bonded investment on its maker's burnout schedule, then clear it with a fluoric-based investment remover; strong acid attacks the cast surface.
- #943 or #940? Both are United white alloys for 10K and 14K. #943 brings 28% silver and pours much cooler; #940 has no silver, a little more nickel (17.6% against 16%) and is made for open melting systems.
Need help choosing?Tell us what you’re making and we’ll point you to the right size and item number.