Skip to product information
Item no. 10-496-50Sold by quote
Medium White Casting Alloy (9K-14K)
Price on request
Shipped across CanadaBy courier or freight: we quote delivery with your price.
Features
All the details- For open meltingUnited formulates #940 for open melting systems, apart from the alloys it makes for enclosed casting machines.
- Copper, zinc and nickel, no silverThis alloy contains 61.40% copper, 21.00% zinc and 17.60% nickel, making it a low-nickel white alloy.
- As-cast hardnessOf 142 HV at 10K and 157 HV at 14K, by United's figures.
- Remelts with half fresh metalUnited calls for a 50% fresh mix, and 15-20 minutes before you quench the flask.
#940 is United Precious Metal Refining's medium white master alloy for 10K and 14K white casting gold. United makes it for open melting systems and describes it as low in nickel; it is a copper, zinc and nickel alloy with no silver. Sold by weight as grain, from 50 g to 1 kg.
Casting reference by karat (United PMR data)
| Karat | Fine gold + #940, per 100 g | Casting temperature | Density | As-cast hardness |
|---|---|---|---|---|
| 10K | 41.7 g + 58.3 g | 1,065-1,085 °C (1,949-1,985 °F) | 11.22 g/cc | 142 HV |
| 14K | 58.5 g + 41.5 g | 1,015-1,035 °C (1,859-1,895 °F) | 12.74 g/cc | 157 HV |
Fine-gold weights follow standard fineness: 417 for 10K, 585 for 14K.
| Maker | United Precious Metal Refining |
|---|---|
| Product code | 940 |
| Colour | Medium white |
| Karat range | 10K-14K |
| Form | Alloying grain |
| Use | Investment casting, open melting systems |
| Composition | Copper 61.40%, zinc 21.00%, nickel 17.60%, silver 0% (published figures; United adds proprietary metals it doesn't list) |
| Pre-alloying | 1,080-1,090 °C (1,976-1,994 °F) |
| Flask temperature | 540-675 °C (1,004-1,247 °F) |
| Quench and remelt | Quench after 15-20 minutes; remelt with 50% fresh metal |
| Sold as | By weight: 50 g, 100 g, 500 g or 1 kg |
| Made in | USA |
Sold as
By weight: 50 g, 100 g, 500 g or 1 kg of #940 alloy grain. No fine gold, flux or investment included.
Good to know
- This is the alloy, not the gold: you melt it with fine gold to reach your karat. For 100 g of 14K, that is 58.5 g of fine gold and 41.5 g of #940.
- Work out the metal from the wax: multiply the alloy's density by the wax pattern's weight in grams, then add 10% for the button. At 14K the density is 12.74 g/cc.
- Keep the flux to a pinch: a little boric acid is all United calls for. It rules out carbon-based fluxes such as soda ash and saltpetre, and a bottom-pour automatic caster needs none at all.
- Investing and devesting: use a gypsum-bonded investment on its maker's burnout schedule, then clear it with a fluoric-based investment remover; strong acid attacks the cast surface.
- #940, #943 or #952? All three are United white alloys we carry for 10K and 14K. #940 is the silver-free choice for open melting; #943 adds 28% silver and casts 170-230 °C cooler; #952 is United's silver-based, high-fluidity alloy for stone-in-place work.
Need help choosing?Tell us what you’re making and we’ll point you to the right size and item number.