Skip to product information
Item no. 10-463-50Sold by quote
Greenish Yellow Casting Alloy (9K-14K)
Price on request
Shipped across CanadaBy courier or freight: we quote delivery with your price.
Features
All the details- Greenish yellow, 9K-14KUPMR's general-purpose casting alloy for this karat range.
- High fluidity for stone-in-place castingFlows cleanly around set stones, per UPMR.
- Harder as cast156 HV at 10K, 174 HV at 14K, UPMR's own figures.
- Needs very little fluxIt also needs only a fluoric-based investment remover, not an aggressive acid.
- Not the same alloy as our Centrifugal/HPS casting alloy(14251): #278 carries more silver and casts harder; #450 is formulated specifically for centrifugal and hand-pouring machines.
Alloy #278 from United Precious Metal Refining (UPMR) is a greenish yellow master alloy for casting 9K to 14K gold, formulated for high fluidity and tarnish resistance. It suits stone-in-place work, where the metal has to flow cleanly around set stones, and can be remelted with up to 50% fresh alloy. Sold by weight in 50 g, 100 g, 500 g and 1 kg.
Melting and casting reference (UPMR data)
| Karat | Pre-alloying °C (°F) | Casting °C (°F) | Density (g/cc) | As-cast hardness (HV) |
|---|---|---|---|---|
| 10K | 1,010–1,040 (1,850–1,910) | 930–950 (1,706–1,742) | 11.31 | 156 |
| 14K | 1,010–1,040 (1,850–1,910) | 920–940 (1,688–1,724) | 12.83 | 174 |
From UPMR's technical sheet for Alloy 278; not the page's own size options, which are by weight, not karat.
| Maker | United Precious Metal Refining (UPMR) |
|---|---|
| Karat range | 9K–14K |
| Colour | Greenish yellow |
| Use | Casting (general purpose, stone-in-place) |
| Composition | Cu 65%, Ag 18%, Zn 17%, Ni 0% |
| Melting range | 920–950 °C (1,688–1,742 °F) casting; 1,010–1,040 °C (1,850–1,910 °F) pre-alloying |
| Alloying ratio | 375 g fine gold + 625 g alloy per kg (9K); 585 g fine gold + 415 g alloy per kg (14K) |
| Sold as | 50 g, 100 g, 500 g or 1 kg of alloy grain |
| Made in | USA |
Sold as
By weight: 50 g, 100 g, 500 g or 1 kg of alloy grain. No gold, flux or investment included.
Good to know
- Flux sparingly: a little boric acid is enough; skip carbon-based flux, and a bottom-pour automatic caster needs none at all.
- Investment: gypsum-bonded, cleared with a fluoric-based remover rather than an aggressive acid, which can corrode the surface.
- Sizing a pour: alloy density (g/cc) × wax pattern weight (g), plus 10% for the button.
- Quench 20–25 minutes after casting; remelt scrap with 35–50% fresh alloy.
- Choosing between #278 and #450: pick this one for general 9K-14K stone-in-place casting; pick the Centrifugal/HPS alloy for centrifugal or hand-pouring machines.