Skip to product information
Item no. 10-474-50Sold by quote
Greenish Yellow Casting Alloy (9K-14K)
Price on request
Shipped across CanadaBy courier or freight: we quote delivery with your price.
Features
All the details- Low in silverT3 is 72.0% copper, 23.0% zinc and just 5.0% silver, compared with 18% silver in United #278 greenish yellow alloy.
- Tarnish resistant and reusableUnited rates T3 for both.
- Softer as cast122 HV at 10K and 134 HV at 14K by United's figures, against 156 and 174 HV for #278.
- One alloy from 9K to 14KT3 has one casting range for 9K-10K and another for 14K, so the same grain covers the whole span.
T3 is United Precious Metal Refining's greenish yellow master alloy for casting 9K to 14K gold: melt it with fine gold, then cast as usual. It is a low-silver alloy, mostly copper and zinc, that United makes to resist tarnish and to stand up to repeated remelting. Sold by weight as alloy grain, from 50 g to 1 kg.
Casting reference by karat (United PMR data)
| Karat | Fine gold + T3, per 100 g | Casting temperature | Density | As-cast hardness |
|---|---|---|---|---|
| 9K | 37.5 g + 62.5 g | 955-975 °C (1,751-1,787 °F) | — | — |
| 10K | 41.7 g + 58.3 g | 955-975 °C (1,751-1,787 °F) | 11.02 g/cc | 122 HV |
| 14K | 58.5 g + 41.5 g | 935-955 °C (1,715-1,751 °F) | 12.56 g/cc | 134 HV |
Density and hardness are shown for 10K and 14K only. Fine-gold weights follow standard fineness: 375 for 9K, 417 for 10K, 585 for 14K.
| Maker | United Precious Metal Refining |
|---|---|
| Product code | T3 |
| Colour | Greenish yellow |
| Karat range | 9K-14K |
| Form | Alloying grain |
| Use | Investment casting |
| Composition | Copper 72.0%, zinc 23.0%, silver 5.0%, nickel 0% (published figures; United adds proprietary metals it doesn't list) |
| Pre-alloying | 1,030-1,065 °C (1,886-1,949 °F) |
| Flask temperature | 510-650 °C (950-1,202 °F) |
| Quench and remelt | Quench after 15 minutes; remelt with 35-50% fresh metal |
| Sold as | By weight: 50 g, 100 g, 500 g or 1 kg |
| Made in | USA |
Sold as
By weight: 50 g, 100 g, 500 g or 1 kg of T3 alloy grain. No fine gold, flux or investment included.
Good to know
- This is the alloy, not the gold: you melt it with fine gold to reach your karat. For 100 g of 14K, that is 58.5 g of fine gold and 41.5 g of T3.
- Work out the metal from the wax: multiply the alloy's density by the wax pattern's weight in grams, then add 10% for the button. At 14K the density is 12.56 g/cc.
- Keep the flux to a pinch: a little boric acid is all United calls for. It rules out carbon-based fluxes such as soda ash and saltpetre, and a bottom-pour automatic caster needs none at all.
- Investing and devesting: use a gypsum-bonded investment on its maker's burnout schedule, then clear it with a fluoric-based investment remover; strong acid attacks the cast surface.
- T3 or #278? Both are United greenish yellow alloys for 9K-14K. T3 is the low-silver, softer-casting, reusable choice; #278 carries more silver, casts harder and is the alloy to use for stone-in-place work.
Need help choosing?Tell us what you’re making and we’ll point you to the right size and item number.