All the details- Made for whitenessUnited's own note for #907 is excellent whiteness, leaving rhodium plating as an option rather than a must.
- Nickel-based, no silver40.0% copper, 40.0% nickel and 20.0% zinc on United's May 2026 sheet.
- Hard as cast215 HV at 14K and 233 HV at 18K, by United's figures.
- Remelt with mostly fresh metalUnited calls for 70% fresh alloy in the crucible when you reuse buttons and sprues.
#907 is United Precious Metal Refining's premium white master alloy for 14K and 18K white casting gold: melt it with fine gold and cast as usual. United rates it for excellent whiteness, with rhodium plating optional. It is a nickel-based alloy with no silver, sold by weight as grain from 50 g to 1 kg.
Casting reference by karat (United PMR data)
| Karat | Fine gold + #907, per 100 g | Casting temperature | Density | As-cast hardness |
|---|---|---|---|---|
| 14K | 58.5 g + 41.5 g | 1,055-1,075 °C (1,931-1,967 °F) | 12.60 g/cc | 215 HV |
| 18K | 75.0 g + 25.0 g | 1,010-1,030 °C (1,850-1,886 °F) | 14.64 g/cc | 233 HV |
Fine-gold weights follow standard fineness: 585 for 14K, 750 for 18K.
| Maker | United Precious Metal Refining |
|---|---|
| Product code | 907 |
| Colour | Premium white |
| Karat range | 14K-18K |
| Form | Alloying grain |
| Use | Investment casting |
| Composition | Copper 40.0%, nickel 40.0%, zinc 20.0%, silver 0% (published figures; United adds proprietary metals it doesn't list) |
| Pre-alloying | 1,080-1,090 °C (1,976-1,994 °F) |
| Flask temperature | 540-675 °C (1,004-1,247 °F) |
| Quench and remelt | Quench after 15 minutes; remelt with 70% fresh metal |
| Sold as | By weight: 50 g, 100 g, 500 g or 1 kg |
| Made in | USA |
Sold as
By weight: 50 g, 100 g, 500 g or 1 kg of #907 alloy grain. No fine gold, flux or investment included.
Good to know
- This is the alloy, not the gold: you melt it with fine gold to reach your karat. For 100 g of 18K, that is 75 g of fine gold and 25 g of #907.
- Work out the metal from the wax: multiply the alloy's density by the wax pattern's weight in grams, then add 10% for the button. At 18K the density is 14.64 g/cc.
- Keep the flux to a pinch: a little boric acid is all United calls for. It rules out carbon-based fluxes such as soda ash and saltpetre, and a bottom-pour automatic caster needs none at all.
- Investing and devesting: use a gypsum-bonded investment on its maker's burnout schedule, then clear it with a fluoric-based investment remover; strong acid attacks the cast surface.
- #907 or #915? Both are United premium white alloys for 14K-18K casting, and neither contains silver. #907 carries more nickel (40% against 30.5%) and is the one United describes for whiteness; #915 is its pick for reusability and surface lustre.
Need help choosing?Tell us what you’re making and we’ll point you to the right size and item number.