Item no. 10-495-50Sold by quote
Medium White Fabricating Alloy (9K-18K)
Price on request
Shipped across CanadaBy courier or freight: we quote delivery with your price.
Features
All the details- Built for working, not castingUnited rates #866 for wire, sheet and plate stock, made by ingot casting and then rolled or drawn.
- Covers the full range we stock it forOne alloy spans 9K through 18K white gold.
- Nickel/zinc-based with no declared silver in the mix
- Annealing window is specific732°C (1350°F) for 20 minutes — over-annealing causes grain growth and an orange-peel surface.
European Design's #866 Medium White is United Precious Metal Refining's master alloy for fabricating 9K to 18K white gold: melt it with fine gold, then roll or draw the ingot into wire, sheet or plate. Unlike our casting-grade white alloys, #866 is built for mechanical working, not lost-wax casting.
Mixing ratio by karat
| Karat | Fine gold (by weight) | Master alloy (by weight) |
|---|---|---|
| 9K | 37.5% | 62.5% |
| 14K | 58.5% | 41.5% |
| 18K | 75.0% | 25.0% |
Fine-gold percentages are standard karat fineness, independent of the alloy maker.
Works with
- Reversible Ingot Mould Wire/Flat
- Ceramic Casting Crucible
| Maker | United Precious Metal Refining |
|---|---|
| Karat range | 9K-18K |
| Colour | Medium white |
| Use | Fabrication — wire, sheet and plate, by ingot casting |
| Composition | Copper 65.00%, zinc 20.00%, nickel 15.00% (nickel-based; no silver) |
| Melting range | 1,060-1,070°C (1,940-1,958°F) initial; 1,010-1,050°C (1,850-1,922°F) ingot, by karat |
| Alloying ratio | 37.5% fine gold for 9K, 58.5% for 14K, 75.0% for 18K, by weight |
| Sold as | By weight, 50 g - 1,000 g (1 kg) |
Sold as
By weight: order 50 g, 100 g, 500 g or 1,000 g (1 kg) of alloy grain. Fine gold is not included — melt it in yourself to reach the karat you need.
Good to know
- Cast the ingot with fine gold on top: melt the alloy in the bottom of the crucible, fine gold on top, for a good mix before pouring into a preheated iron mould — a round rod mould for wire, a 2-piece L-shaped mould for sheet or plate.
- Quench heavy ingots carefully: let them cool about a minute before quenching in pickle solution or water, to avoid quench cracking.
- Roll or draw in 50% steps, cleaning the ingot and annealing at 732°C (1,350°F) for 20 minutes between passes; keep rolls and dies clean to avoid surface defects.
- Don't over-anneal: it causes excessive grain growth and an orange-peel surface. A boric acid fire coat protects the surface when annealing in open air.
- Don't confuse this with our casting-grade white alloys: #915 and #930 are formulated for lost-wax casting; #866 is built for mechanical working into wire, sheet and plate.
Need help choosing?Tell us what you’re making and we’ll point you to the right size and item number.