Skip to product information
Item no. 52-591-5In stock
U-NAMEL Coloured UV-Curing Enamels
$16.50
Features
All the details- Cures in 1-2 minutesUnder a UV lamp, instead of firing in a kiln.
- Machinable once curedDrill, grind, polish, carve or sand it, and it can be turned on a lathe.
- Layer it to build up colour or cabochonsIncluding over previously cured U-Namel.
- Adheres to metal, stone, glass, plastic, ceramic and fired enamel
- Metal around it can still be electroplatedAfterward without affecting the cured enamel.
U-Namel is a UV-light-curing coloured enamel: apply it wet, then harden it in 1-2 minutes under a UV lamp, no kiln needed. It comes in 8 opaque colours, cures hard enough to drill, grind, carve or polish, and can be layered to build up cabochons.
| Maker | JSP (U-Namel) |
|---|---|
| System | UV-curing enamel (light-sensitive resin, not a fired glass enamel) |
| Cure time | 1-2 minutes under a UV curing light |
| Layer thickness | About 0.2 mm for dark colours; about 0.8 mm for clear or light colours |
| Storage | 15-21 °C (59-70 °F), out of light, in the bottle provided |
| Shipping | Non-hazardous; ships by air |
Sold as
Each: one squeeze bottle of one colour, labelled 15 g by the maker. Not included: a UV curing light, primer, or application tools.
Good to know
- Prep the surface first: roughen or lightly sandblast it (150-250 micron abrasive at 60-90 psi) and degrease it; apply U-Namel at room temperature.
- Thin coats cure best: about 0.2 mm for dark colours and 0.8 mm for clear or light colours. Thicker layers take longer to cure and may not harden all the way through.
- Changing your mind on a piece? Our U-NAMEL® Blaster-Remover breaks up cured U-Namel in about a minute. You can also grind it off or burn it off at 300-380 °C.
- Want a transparent look instead? See our U-NAMEL® Transparent Coloured UV-Curing Enamels.
The enamel itself is non-hazardous and ships by air. The main hazard is the UV curing lamp: looking directly into an uncovered lamp without amber, UV-rated goggles can cause severe eye damage.
Need help choosing?Tell us what you’re making and we’ll point you to the right size and item number.