Standard Yellow (9K-14K) Rolling Alloy
Price on request
Shipped across CanadaBy courier or freight: we quote delivery with your price.
Features
All the details- Built for fabrication, not castingUPMR rates #820 for rolling, drawing and stamping wire, sheet and plate, not for pouring into a mould.
- Low silver, lightweightA light, low-silver alloy suited to wire and stamping work.
- Documented rolling schedule50% size reduction between anneals, annealed at 675 °C (1,250 °F) for 20 minutes.
- Melt gold on top of the alloyPer UPMR, then pour into a round mould for wire or an L-shaped mould for plate and sheet.
- Sold by weight100 g, 500 g and 1 kg.
Alloy #820 from United Precious Metal Refining (UPMR) is a low-silver, lightweight standard yellow master alloy built for fabricating 9K to 14K gold: rolling, drawing and stamping wire, sheet and plate. UPMR files it separately from its casting alloys, with its own melting, rolling and annealing schedule. Sold by weight in 100 g, 500 g and 1 kg.
| Maker | United Precious Metal Refining (UPMR) |
|---|---|
| Karat range | 9K–14K |
| Colour | Standard yellow |
| Use | Fabrication (rolling, wire and sheet) |
| Composition | Cu 73%, Ag 12%, Zn 15%, Ni 0% |
| Melting range | 950–980 °C (1,742–1,796 °F) ingot pour; 1,040–1,050 °C (1,904–1,922 °F) initial melt |
| Alloying ratio | 375 g fine gold + 625 g alloy per kg (9K); 585 g fine gold + 415 g alloy per kg (14K) |
| Sold as | 100 g, 500 g or 1 kg of alloy grain |
| Made in | USA |
Sold as
By weight: 100 g, 500 g or 1 kg of alloy grain. No gold included.
Good to know
- Melting order: alloy in the bottom of the crucible, fine gold on top; melt, then let the temperature drop to the ingot-pouring range before pouring.
- Choose your mould: a round rod mould for wire, a 2-piece L-shaped mould for plate and sheet, both preheated and lightly lubricated.
- Quench promptly, but let a heavy ingot air-cool about a minute first to avoid quench cracking.
- Work in 50% reductions between anneals, cleaning the stock after each one; keep rolls and dies clean to avoid surface defects.
- Don't over-anneal: 675 °C (1,250 °F) for 20 minutes, then quench. Longer or hotter causes grain growth and an orange-peel surface; apply a boric acid fire coat first if annealing in open air.