Skip to product information
Item no. 10-480-50Sold by quote
Premium White Casting Alloy (14K-18K)
Price on request
Shipped across CanadaBy courier or freight: we quote delivery with your price.
Features
All the details- High reusabilityUnited formulates #915 to keep its surface lustre through repeated remelts, recommending a 70% fresh mix when reworking flask buttons and sprues.
- Two casting windows1,030-1,050°C (1,886-1,922°F) for 14K and 1,000-1,025°C (1,832-1,877°F) for 18K, with a 15-30 minute quench.
- High nickel content30.50% nickel, the most of any white alloy we stock, with no palladium or extra silver in the mix.
- Straightforward flux and investmentVery little boric acid flux, a gypsum-bonded investment, and a fluoric-based investment remover for the silicon-oxide surface coating.
European Design's #915 Premium White is United Precious Metal Refining's master alloy for 14K and 18K white casting gold: melt it with fine gold and cast as usual. United rates it for high reusability and surface lustre, and it carries the highest nickel content of the white alloys we stock.
Mixing ratio and properties by karat (United Precious Metal Refining)
| Karat | Fine gold (by weight) | Master alloy (by weight) | Density (g/cc) | As-cast hardness (HV) |
|---|---|---|---|---|
| 14K | 58.5% | 41.5% | 12.57 | 195 |
| 18K | 75.0% | 25.0% | 14.61 | 231 |
Fine-gold percentages are standard karat fineness; density and hardness are United's own figures for Alloy 915.
| Maker | United Precious Metal Refining |
|---|---|
| Karat range | 14K-18K |
| Colour | Premium white |
| Use | Casting |
| Composition | Copper 49.50%, zinc 20.00%, nickel 30.50% (nickel-based; no silver) |
| Melting range | 1,060-1,070°C (1,940-1,958°F) pre-alloying; 1,000-1,050°C (1,832-1,922°F) casting, by karat |
| Alloying ratio | 58.5% fine gold for 14K, 75.0% for 18K, by weight |
| Sold as | By weight, 50 g - 1,000 g (1 kg) |
Sold as
By weight: order 50 g, 100 g, 500 g or 1,000 g (1 kg) of alloy grain. Fine gold is not included — melt it in yourself to reach the karat you need.
Good to know
- Weigh by density, not guesswork: multiply the alloy's density (12.57 g/cc for 14K, 14.61 for 18K) by your wax pattern's weight to estimate the metal needed, then add 10% for the button.
- Keep the flux light: very little boric acid is enough; avoid carbon-based fluxes like soda ash or saltpetre, and skip flux altogether in a bottom-pour automatic caster.
- Match your investment remover to the alloy: a fluoric-based remover suits #915's silicon-oxide surface coating, since aggressive acid can corrode and mark the surface.
- Don't confuse this with our other white alloys: #930 Ultra White (9K-18K, lower nickel) and Legor's white working alloy are different formulations for different karat ranges and uses.
Need help choosing?Tell us what you’re making and we’ll point you to the right size and item number.